Recovery of iron from vanadium tailings with coal-based

A technique with coal-based direct reduction followed by magnetic separation is presented in this study for recovering and reusing iron otherwise wasted in vanadium tailings. Process parameters such as usage of additives, tailings/reductant/additives ratio, reduction temperature and time, as well as particle size were experimentally determined.

More

Iron recovery from zinc mine tailings by magnetic

Considering the whole process, magnetic separation and carbothermal reduction, the recovery of Fe from the zinc mine tailings was 67%. Therefore, the process route suggested in this study will not only reduce tailings disposal and consequently the risk of environmental accidents, but it will also provide profitable raw material for the steel

More

Recovery of iron from cyanide tailings with reduction

In this paper, recovery of iron from cyanide tailings was studied with reduction roasting-water leaching process followed by magnetic separation. After analysis of chemical composition and crystalline phase, the effects of different parameters on recovery of iron were chiefly introduced.

More

Recovery of iron from hazardous tailings using fluidized

Feb 01, 2020· Much recently, Yu et al. indicated the technical realizability of fluidized magnetization roasting with low-intensity magnetic separation technology for separating iron from the magnetic preconcentrates of iron ore tailings; a concentrate with an iron grade of 61.4% and recovery of 81.8% was obtained under the optimum conditions .

More

Iron recovery from zinc mine tailings by magnetic

The Canadian Journal of Chemical Engineering, published by Wiley on behalf of The Canadian Society for Chemical Engineering, is the forum for publication of high quality original research articles, new theoretical interpretation or experimental findings and critical reviews in the science or industrial practice of chemical and biochemical processes.

More

Efficient iron recovery from iron tailings using advanced

Recycling iron tailings is significant for environmental security and resource recovery, as they contain iron-rich minerals. Given the complex composition of iron minerals and the low grade of iron present in the tailings, innovative suspension roasting-magnetic separation (SRMS) technology was proposed to treat iron tailings that would separate out the iron minerals for recovery.

More

(PDF) Recovery of Ultra-Fine Iron Ore from Iron Ore Tailings

In the second option, the iron ore tail is treated in a similar approach, but the gravity concentration replaced by magnetic separation results in a product quality with 65.34% Fe, 3.70% SiO2 and

More

TAILINGS CHARACTERIZATION OF „CHELOPECHENE”

Magnetic iron concentrate iron content is 49-50%, iron recovery is 68%. Flotation iron concentrate iron content is 37%, iron recovery is 85%. Barite concentrate barium sulphate content is 85%. The final technological tailings (called „black tailings“) are stored at “Chelopechene” Tailings Pond.

More

(PDF) Generation and Treatment of Iron Ore Tailings

Many news technologies are being used t o monitoring tailings pond more tailings disposal and water recovery at iron ore mine. followed by magnetic separation was used to utilize the

More

iron ore recovery from tailing pond

Recovery of iron from hazardous tailings using fluidized. Feb 01, 2020· The recovery of iron from iron ore tailings using magnetic separation after magnetizing roasting J Hazard Mater, 174 (2010), pp 71-77 Google Scholar SK Das, S Kumar, P RamachandraraoExploitation of iron ore tailing for the development of

More

Efficient iron recovery from iron tailings using advanced

Recycling iron tailings is significant for environmental security and resource recovery, as they contain iron-rich minerals. Given the complex composition of iron minerals and the low grade of iron present in the tailings, innovative suspension roasting-magnetic separation (SRMS) technology was proposed to treat iron tailings that would separate out the iron minerals for recovery.

More

Recovery of iron from hazardous tailings using fluidized

Feb 01, 2020· Much recently, Yu et al. indicated the technical realizability of fluidized magnetization roasting with low-intensity magnetic separation technology for separating iron from the magnetic preconcentrates of iron ore tailings; a concentrate with an iron grade of 61.4% and recovery of 81.8% was obtained under the optimum conditions .

More

Iron recovery from zinc mine tailings by magnetic

The Canadian Journal of Chemical Engineering, published by Wiley on behalf of The Canadian Society for Chemical Engineering, is the forum for publication of high quality original research articles, new theoretical interpretation or experimental findings and critical reviews in the science or industrial practice of chemical and biochemical processes.

More

Recycling of iron and titanium resources from early

Geochemical characterization of the tailings was first conducted, followed by the iron recovery and titanium recovery. Iron recovery was mainly achieved through a series of magnetic separation, and titanium recovery was on the combination of magnetic pre-concentration and flotation separation.

More

TAILINGS CHARACTERIZATION OF „CHELOPECHENE”

Magnetic iron concentrate iron content is 49-50%, iron recovery is 68%. Flotation iron concentrate iron content is 37%, iron recovery is 85%. Barite concentrate barium sulphate content is 85%. The final technological tailings (called „black tailings“) are stored at “Chelopechene” Tailings Pond.

More

Magnetic Separation to Recover Iron Minerals from

A joint process of flotation and magnetic separation was proposed to process the ore. This paper introduces the test results of flotation tailings by a wet drum separator. Results show that iron concentrate assaying 60.21-68.12% Fe at a recovery of 71.9-75.32% can be obtained, when the flotation tailings assays 33.91%Fe.

More

[PDF] The Challenge to Scavenge IRON from Tailings

Tailings recovery has been a constant challenge for most engineers. Along more than five years, GAUSTEC joined major players in the mining Industry to scavenge Iron from tailings produced by flotation making use of WHIMS (Wet High Intensity Magnetic Separation). In the early 1980s, in USA, the US 4,192,738 patent was granted with promising results.

More

Innovative Technique to generate saleable Iron Ore Fines

Earlier Iron ore tailings contain iron concentrations of around 45% or more. In on ultra-fines recovery plant tailings revels that, there was an escape of martite, goethite and hematite in tailings. Again an attempt was made in 2010 by wet high intensity magnetic separation. Medium intensity magnetic separation

More

Recovery of Pt and Pd from PGM Mine Tailings by Magnetic

2.2.2 Magnetic separation Recovery of Pt and Pd from PGM Mine Tailings by Magnetic Separation Jan Pana RABATHO, William TONGAMP, Yasushi TAKASAKI and Atsushi SHIBAYAMA Faculty of Engineering and Resource Science, Akita University, Tegata-Gakuen-cho, Akita 010-8502, Japan E-mail: [email protected] (J.P. Rabatho)

More